AOI Optical Inspection

AOI Optical InspectionPackage surface defects, glass edge chipping and edge grinding measurement, with lighting and algorithms tuned to your defects

AOI (Automated Optical Inspection) uses cameras and lighting to capture images, then image-processing algorithms to judge defects. We develop our own lighting optics, imaging and algorithms. For assembly and test, it inspects surface defects such as scratches, mold flash and edge press marks, front and back at the same time. For panels and glass carriers, it handles edge chipping and crack inspection, cut-face depth measurement and real-time edge grinding measurement, and is in production at 6 sites of a major Taiwanese panel maker.

Front & backInspected at the same time
Mono/multispectralLighting chosen per defect
SubPixelSub-pixel measurement
6 sitesLive at panel fabs
AOI color image: defects on an IC package surface
Actual images from package surface inspection.
EEnvironmentalSSocial

ESG positioning: E (Environmental) + S (Social)SDG 9Industry & InnovationSDG 12Responsible ProductionHow DEYly approaches ESG →

Proven benefits
Automatic defect detection reduces scrap and rework from defective parts reaching downstream processes (E); long hours of microscope inspection move to AOI, and staff shift to review and process improvement (S).
Limits
Detection and overkill rates depend on defect type, imaging conditions and judgment thresholds. Before deployment we evaluate by imaging your actual samples rather than promising generic numbers.

Packaging inspectionWhich surface defects can AOI inspect in assembly and test?

Depending on customer needs, it can inspect defects such as scratches, mold flash and edge press marks, front and back at the same time. Whether to use monochrome or color imaging, and single-wavelength or multispectral lighting, is decided by imaging actual samples first; only then do we choose the optical path and camera.

AOI monochrome image: mold marks and scratches on an IC surface
Mold marks/scratchesMonochrome image marking the locations of mold marks and scratches.
AOI monochrome image: scratch on an IC surface
ScratchA long, thin surface scratch boxed in.
AOI monochrome image: fine scratch on an IC surface
Fine scratchA thin-line scratch in the center area.
AOI monochrome image: leadframe edge press mark measurement
Edge press markPress mark on the leadframe edge, with the measured value labeled alongside.

Images come from actual assembly and test samples; inspection items and judgment criteria are built on the customer's defect definitions.

LightingWhy choose lighting by defect?

On the same IC, change the lighting and the defect contrast changes completely. Some defects are clearest under single-wavelength light; others need multispectral lighting to tell materials apart. So our first step in AOI isn't writing code but designing the lighting and optical path: reflection, folding and loss, angle of incidence and wavelength, and finally an imaging evaluation.

The same type of defect imaged under single-wavelength lighting
Single-wavelength imagingClear contrast between the defect area and the background.
The same type of defect in color images under different spectra
Multispectral imagingUnder different spectra, defects show up in different colors, helping distinguish materials.

Glass inspection modulesWhat can be inspected and measured on panel glass?

The glass inspection modules are installed on panel lines for real-time inspection. They are currently in use at 6 sites of a major Taiwanese panel maker, at a Japanese panel maker, and on wafer glass carriers for assembly and test.

Three glass inspection modules
ModuleWhat it inspectsTrack record
Glass edge chipping inspectionInspects along the glass edge for chipping; crack inspection can be added3 sites of a major Taiwanese panel maker, a Japanese panel maker, wafer glass carriers
Glass cut-face depth measurementMeasures the depth of the cut face after cutting4 sites of a major Taiwanese panel maker
Real-time glass cutting and edge grinding measurementFront: multi-point edge grinding measurement along edges, dual-edge measurement at corners, edge chipping at corners and edges; back: multi-point edge grinding measurement at corners and edges, dual-edge measurement at corners, edge chipping at corners and edges2 sites of a major Taiwanese panel maker
Image of glass edge chipping
Edge chippingChips on the glass edge are clearly visible under backlight.
Image of a glass crack
Crack inspectionA long, thin crack extending from the edge.
Glass inspection module installed on the production line
Inspection moduleCamera and lighting modules mounted above the line.
Glass cut depth measurement module installed on a roller conveyor
Cut depth measurementThe module is mounted on a roller conveyor and measures the glass in real time as it passes.
Glass corner edge grinding measurement screen: green measurement lines
Edge grinding measurement (front)Multi-point measurement at corners and edges; the green line is the measurement reference.
Glass back-side corner edge grinding measurement screen
Edge grinding measurement (back)Dual-edge measurement at the back corners.

Software & algorithmsHow are the AOI software and algorithms built?

Software platform and algorithms
ItemDetailsWhy we do it this way
Development platformLinux x86 (primary), Windows x86, Linux ARMLinux suits long-running operation: system updates and hardware changes have little impact, and it is less prone to malware
Programming languageC/C++, with critical computations accelerated in assembly and SSE, AVX and NEON instructionsThe same code runs across platforms, reducing duplicate development and knowledge gaps
Algorithm coreImage structures based on OpenCV, with basic algorithms optimized for speed in assemblyFast enough to keep up with the line's takt time
In-house advanced algorithmsImage alignment, image subtraction, neighbor subtraction, SubPixel vision measurement, SubPixel object detection and morphology analysis (Blob/Object)Tunable to customer defects, not limited by packaged software
Lighting and optical path designReflection, folding, loss; angle, wavelength; imaging evaluationCapture the defect clearly first, and the algorithm can judge it accurately

SubPixel measurement uses grayscale changes at image edges to compute positions finer than a single pixel, so the same camera measures more precisely.

How we startHow do you get started with AOI?

  1. 01Provide samplesGood parts plus samples of each defect type; the more variety, the better
  2. 02Imaging evaluationTest lighting: monochrome or color, single-wavelength or multispectral
  3. 03Build judgment rulesAlgorithms and thresholds built on your defect definitions
  4. 04In-line validationCompare with manual judgment; tune escapes and overkill
  5. 05Go liveResults and images uploaded to the system, with ongoing tuning

SpecificationsSpec

Main specifications
Inspection targetsIC package surfaces, leadframes; panel glass, glass carriers
Package defectsScratches, mold flash, edge press marks and more, per customer definitions
Inspection surfacesFront and back inspected at the same time
ImagingMonochrome or color, confirmed by imaging actual samples
LightingSingle-wavelength or multispectral, chosen per defect
Glass inspectionEdge chipping, cracks, cut-face depth, real-time edge grinding measurement
MeasurementSubPixel vision measurement, SubPixel object detection and morphology analysis
Software platformLinux x86 (primary), Windows x86, Linux ARM
Programming languageC/C++, SSE, AVX and NEON acceleration

AOI is customized to the inspection target; detection capability is confirmed after an imaging evaluation with actual samples.

FAQCommon questions

What is AOI?

AOI (Automated Optical Inspection) uses cameras and lighting to capture images, then image-processing algorithms to judge defects or measure dimensions, replacing manual visual inspection.

Which IC package defects can AOI inspect?

Depending on customer needs, it can inspect surface defects such as scratches, mold flash and edge press marks, front and back at the same time. Inspection items and judgment criteria are built on the customer's defect definitions.

Why send samples first?

The same defect can show very different contrast under different lighting. We first test lighting and imaging methods (monochrome, color, single-wavelength or multispectral) on actual samples to make sure the defect is captured clearly; that is what lets the algorithm judge accurately.

What can the glass inspection modules do?

They handle glass edge chipping and crack inspection, cut-face depth measurement, and real-time cutting and edge grinding measurement (multi-point edge and dual-edge corner measurement, front and back). They are in production at 6 sites of a major Taiwanese panel maker.

What is SubPixel measurement?

Sub-pixel measurement uses grayscale changes at image edges to compute positions finer than a single pixel, so the same camera resolution measures more precisely.

How do you balance AOI escapes and overkill?

An escape is a defective part that gets passed; overkill is a good part misjudged as defective. The two pull against each other. At deployment we compare results against manual judgment on actual samples, tune the thresholds, then set the acceptance standard.

Can I buy directly from DEYly? Who handles quotations and after-sales service?

Yes. This equipment is sold by DEYly, and DEYly handles both quotations and after-sales service. Before quoting, we evaluate your products, throughput and line conditions. You can send your requirements directly through the inquiry form.

Let's talk

Problems on site: assess first, then decide

Tell us about your equipment, line and what you're seeing. We'll understand the situation first, then give an initial assessment and recommended options.