Industry News・Supercritical Drying

The TSMC 2nm chip in iPhone 18 Pro: why is even “drying” a challenge for suspended nanosheets? How supercritical CO₂ drying works

A teardown of the iPhone 18 Pro, with the chip cross-sectioned and examined under an electron microscope, confirmed that TSMC's 2nm process already uses GAA nanosheet transistors. During fabrication, these transistors are a few silicon sheets suspended in mid-air, with gaps of less than 10 nm between them. The biggest risk may not be making them but drying them: as the water dries, surface tension can pull the sheets together until they stick. This article explains how this happens, why supercritical CO₂ drying solves it, how it's done on site, and which structures are worth it.

4:01 video: how nanosheets are made, how a little water in the gaps can ruin a transistor, and the principle, history and four on-site steps of supercritical CO₂ drying.

4:47 video: how nanosheets are made, how a little water in the gaps can ruin a transistor, and the principle, history and four on-site steps of supercritical CO₂ drying.

Summary: why do 2nm nanosheets need supercritical CO₂ drying?

GAA nanosheet transistors are made by stacking silicon and silicon-germanium layer by layer, then removing the SiGe so the silicon sheets are left suspended in mid-air. At the 2nm generation, the gaps between sheets are less than 10 nm. After the SiGe is removed, the wafer is rinsed with water and dried, and surface tension as the water recedes can pull adjacent sheets together. Once they stick, they don't come apart. A common approach is to replace the water with IPA (isopropyl alcohol) before drying, since IPA's surface tension is only about a third of water's. But as structures get taller and gaps narrower, they can still collapse even with IPA. Supercritical CO₂ drying heats and pressurizes CO₂ above its critical point, where there's no liquid surface and therefore no surface tension. The CO₂ dissolves the IPA out of the gaps and is then vented as a gas. For short, wide structures, IPA drying may be enough. Only tall, thin structures with narrow gaps warrant switching to supercritical.

Inside the iPhone 18 Pro chip: nanosheets suspended in mid-air during fabrication

TechInsights tore down the A20 Pro chip in iPhone 18 Pro and confirmed that TSMC's 2nm uses GAA nanosheet transistors, now in volume production and inside phones on the market (Tech Times, 2026-09-23).

How are these transistors made? First, silicon and silicon-germanium are stacked layer by layer, like a mille-feuille. In one approach, chemicals selectively remove the SiGe, leaving the silicon suspended in mid-air, and the gate later wraps around it on all four sides. At the 2nm generation, the gaps between sheets are less than 10 nm, more than ten thousand times thinner than a human hair (a hair is about 80,000–100,000 nm, NNI). For the full front-end process flow, see Semiconductor front-end process flowchart.

How much does losing one 2nm wafer cost? Reportedly about US$30,000 per wafer, or nearly NT$1 million (TrendForce citing supply-chain sources, 2025-10-08; not an official price; converted at about NT$32.7 per US$1).

What the news didn't mention: how can a little water left in the gaps ruin a transistor?

Gray 3D nanosheet structure with the two middle sheets bent inward and stuck together
During drying, adjacent nanosheets can be pulled together and stick (3D illustration)

After the SiGe is removed, the chemicals are rinsed off with water and the wafer is dried. The problem comes at the moment of drying, because water has surface tension. Think of a calligraphy brush: its bristles spread out in water but clump together the moment it's lifted out. In the same way, water receding from between the sheets pulls them inward. Once they bend and touch, they can stick and never separate. The industry calls this stiction or pattern collapse.

This isn't our speculation. In introducing nanosheet transistors, imec noted that stiction must be controlled after nanosheet release to keep these tiny sheets from sticking together (imec, 2022). A SEMI industry presentation also pointed out that nanosheets need surface-tension-free drying after wet cleaning to avoid pattern collapse, and that supercritical CO₂ drying may be one application (SEMI EMG, 2022-03-23). There's no public data on how many wafers production lines actually scrap because of this, so we only say “may.”

  • Taller structures→More surface for the water to pull on and a longer lever arm, so they bend more easily
  • Narrower gaps→Stronger capillary forces, so adjacent structures are more easily pulled together
  • Thinner structures→Softer and easier to bend; once they touch, they may stick

What is supercritical CO₂ drying? No liquid surface, no surface tension

Heat and pressurize carbon dioxide past its critical point (about 31°C and 73.8 bar, NIST), and it's no longer distinctly liquid or gas. Like a gas, it gets into the finest gaps; like a liquid, it dissolves the IPA in those gaps and carries it away. That temperature is lower than body temperature, but the pressure is higher than inside a CO₂ fire extinguisher, so the process has to run in a thick, pressure-rated chamber. For a plain-language illustrated guide to supercritical CO₂, see What is supercritical CO₂.

It works because there's no liquid surface. No liquid surface means no surface tension, so the brush dries without its bristles clumping together.

Three drying methods compared (compiled by DEYly)
Drying methodSurface tensionSuitable structures
Drying directly from waterHigh (baseline)Short, wide structures with wide gaps
Replace water with IPA, then dryAbout a third of water'sModerate aspect ratios; may still collapse as structures shrink further
Supercritical CO₂ dryingNo liquid surface, no surface tensionTall, thin suspended structures with narrow gaps

This technique wasn't originally for chips

  1. 1951: electron microscopy samples

    Thomas Anderson of the University of Pennsylvania published the critical point drying method for drying biological samples for electron microscopy, so that surface tension wouldn't crush the samples as they dried (Microscopy Today).

  2. Early 1990s: MEMS research

    MEMS (micro-electro-mechanical systems) researchers used it to dry suspended structures, solving the problem of cantilevers and membranes sticking to the substrate after release. For why MEMS fears water, see What is MEMS.

  3. 1998: a patent for drying wafers

    A patent was filed for using supercritical CO₂ to dry wafers (US6067728).

  4. Today: advanced nodes

    The taller the structures and the narrower the gaps, the stronger the water's pull. Replacing water with IPA first is common practice, but a 2013 wafer-drying study noted that IPA's surface tension is only about a third of water's and leaves little margin for smaller patterns (ECS Transactions, 2013). That made supercritical drying one of the options.

How is it done on site? The four steps of supercritical CO₂ drying

  1. Step 1: Replace water with IPA

    After the chemicals are rinsed off with water, the water is first replaced with IPA (isopropyl alcohol). Water and carbon dioxide don't mix, but supercritical CO₂ can dissolve IPA and carry it away.

  2. Step 2: Transfer into the pressure chamber while still wet

    While the wafer is still wet, it goes into a high-pressure chamber. Think of a pressure cooker at dozens of times the pressure. If the wafer dries even a little on the way, the structures can still collapse.

  3. Step 3: Fill with CO₂ and heat and pressurize to supercritical

    Carbon dioxide is pumped in and heated and pressurized above the critical point to dissolve the IPA in the gaps and carry it away.

  4. Step 4: Hold the temperature and vent slowly

    The temperature is held while the pressure is slowly reduced. The CO₂ leaves directly as a gas without passing through the liquid phase, and the wafer is dry.

How do you tell if drying is the problem? Which structures are worth supercritical drying?

After drying, cross-section the wafer and check whether adjacent structures have collapsed or stuck together. If the structures aren't tall and the gaps aren't narrow, IPA drying may be enough. Only tall, thin structures with narrow gaps warrant switching to supercritical.

How we recommend choosing a drying method (compiled by DEYly)
WorkpieceRecommendationReason
Advanced-node wafers (suspended structures such as nanosheets)Consider supercritical firstNarrow gaps and thin structures carry the highest surface-tension risk
MEMS and sensorsConsider supercritical firstCantilevers and membranes tend to stick to the substrate after release
R&D samplesConsider supercritical firstFew samples and new structures; rule out drying as a variable first
Workpieces with short, wide structures and wide gapsTry IPA drying firstLow surface-tension risk; saves cost and time

Check how tall the structures are and how narrow the gaps are before choosing a drying method. That's the most cost-effective approach. For why 2nm cleaning keeps getting harder, see 2nm wafer cleaning. To test with your own samples before deciding, see Cleaning trial evaluation.

FAQ

Why do nanosheets stick together when 2nm chips are dried?

Nanosheets are suspended in mid-air during fabrication, with gaps of less than 10 nm between them. As the water dries, surface tension pulls adjacent sheets inward, and once they bend and touch they can stick permanently. The industry calls this stiction or pattern collapse.

What is supercritical CO₂ drying?

CO₂ is heated and pressurized above its critical point (about 31°C and 73.8 bar), where it's no longer distinctly liquid or gas. It dissolves the IPA in the gaps, then the pressure is slowly released and the CO₂ is vented as a gas. There's no liquid surface during the process, so there's no surface tension to pull fine structures over.

Isn't IPA drying enough?

IPA's surface tension is only about a third of water's, so IPA drying may be enough for short, wide structures with wide gaps. But tall, thin structures with narrow gaps can still collapse with IPA, and that's when supercritical CO₂ drying is needed.

How do you know a yield problem comes from drying?

After drying, cross-section the wafer and check whether adjacent structures have collapsed or stuck together. If the structures are fine before drying and collapse only afterward, drying is very likely the problem.

Source

  1. Tech Times (citing TechInsights), “TechInsights Teardown Confirms TSMC 2nm Nanosheet Transistors Now Inside iPhone 18 Pro,” 2026-09-23. Link
  2. TrendForce, “[News] TSMC 2nm Reportedly Up 10–20%, Far Below Rumored 50%; 3–7nm to Rise Single-Digit in 2026,” 2025-10-08. Link
  3. imec, “Entering the nanosheet transistor era,” 2022. Link
  4. SEMI EMG, “Logic Transistor Evolution,” 2022-03-23. Link
  5. NIST Chemistry WebBook, “Carbon dioxide: Thermophysical Properties,” accessed 2026-11. Link
  6. Microscopy Today, “History of High Vacuum and Critical Point Equipment Used in EM Specimen Preparation,” accessed 2026-11. Link
  7. Google Patents, “US6067728 Supercritical phase wafer drying/cleaning system,” filed 1998. Link
  8. ECS Transactions, “Advanced Wafer Drying Technology for 1x Node and Beyond Using Surface Modification Method,” 2013. Link
Ask us

Can't find the answer? Ask us directly

Tell us what you're facing. DEYly's engineering and market teams will help assess it and give you initial recommendations.