Key takeaways: What are the photoresist stripping methods and how do they differ?
Photoresist stripping removes the spent photoresist after lithography, etching or ion implantation, and there are three main methods. ① SPM (concentrated sulfuric acid + hydrogen peroxide): wet, breaking down photoresist through hot, strong oxidation; fast and clean, but it requires large amounts of strong acid and high temperatures, and too much heat also etches silicon nitride and silicon oxide films. ② Plasma ashing: dry, turning photoresist into gas with oxygen plasma in a vacuum chamber; no strong acid, but it can leave residue and often needs a follow-up wet clean. ③ Ozone water / ozone microbubbles: wet, oxidizing photoresist with ozone and OH radicals without large amounts of sulfuric acid; research has shown ozone microbubbles increase stripping rates. The hardest case is photoresist after high-dose ion implantation: its surface turns into a carbonized crust that resists ordinary strippers and can burst if heated too fast during ashing, so it is usually removed in stages.
What is photoresist, and why must every layer be stripped?
In one sentence: photoresistWhat is photoresist?A light-sensitive coating that changes its properties when exposed to light, applied as a thin layer on the wafer surface.The exposed areas (or unexposed ones) are washed away by developer, and what remains becomes a “protective film” shaped like the circuit pattern to be made.It is only a temporary tool and must be removed afterward; it cannot stay in the chip.It is like the masking tape you put on a wall before spray painting: stick it on, etch or implant, then peel it off cleanly. Photoresist stripping is the peeling step, and it happens for every layer of the chip.
Coat the wafer evenly with a thin layer of light-sensitive resist.
Print the circuit pattern with light and wash away the unwanted parts, leaving patterned “tape.”
Areas not covered by photoresist are etched away or implanted with ions; covered areas are protected.
The spent photoresist must be completely removed before the wafer can move on to the next layer. Any residue left behind can become a defect.

Photoresist is a light-sensitive material whose properties change on exposure; after development it leaves a patterned protective layer on the wafer surface (Wikipedia: Photoresist). It is only a “tool” in the process, not part of the chip, so it must be fully removed after every etch or implant.
An advanced chip stacks dozens of layers, so the sequence “coat photoresist → lithography → etch/implant → strip → clean” repeats dozens of times. Photoresist stripping may be unglamorous, but it is one of the most frequent steps in front-end processing. See where each station sits in the front-end process flow chart, and the full line in the semiconductor process flow chart.
Three ways to strip photoresist
Method ① Wet
SPMWhat is SPM?Short for Sulfuric acid–Peroxide Mixture: concentrated sulfuric acid plus hydrogen peroxide, known in labs as “Piranha solution.”A common ratio is 3 parts concentrated sulfuric acid to 1 part 30% hydrogen peroxide; mixing releases a lot of heat and can exceed 100 °C.It is extremely oxidizing and corrosive and can “burn off” organics like photoresist, but handling and waste treatment require great care.: “burn it off” with hot strong acid
Wafers are immersed in or sprayed with heated concentrated sulfuric acid + hydrogen peroxide. The strong oxidizing power rapidly breaks down organics like photoresist; it is the most traditional and most widely used stripping method.
Strength: fast, thorough | Cost: large volumes of strong acid, high heat and waste
Method ② Dry
Plasma ashingWhat is ashing?A dry stripping method that uses plasma to “burn” photoresist into gas and pump it away.Highly reactive oxygen atoms in the plasma react with the photoresist to form ash-like gaseous products, which a vacuum pump removes, hence the name “ashing.”No liquids are used; wafers go in and come out dry.: turn photoresist into gas with plasma
Oxygen and other gases are fed into a vacuum chamber and energized into plasma; reactive oxygen atoms react with the photoresist and the resulting gas is pumped away. Many tools generate the plasma remotely and let only the reactive species drift onto the wafer, reducing damage from charged particles.
Strength: dry, no strong acid | Cost: may leave residue, often needs a follow-up wet clean
Method ③ Wet (greener)
Ozone water / ozone microbubbles: oxidative decomposition
Ozone is dissolved in pure water and sprayed onto the spinning wafer. Ozone and the OH radicals it generates in waterWhat are OH radicals?A small molecule of one oxygen and one hydrogen missing an electron; it grabs electrons from other molecules and breaks down organics, reacting away as soon as it forms and leaving no residue.See the full illustrated explanation → oxidize the photoresist; adding microbubbles raises the dissolved ozone concentration and speeds up stripping.
Strength: little sulfuric acid, low residue | Cost: requires ozone safety and exhaust treatment
All images are AI-generated illustrations
A common SPM ratio is 3 parts concentrated sulfuric acid to 1 part 30% hydrogen peroxide; mixing releases so much heat that it can exceed 100 °C on its own (Wikipedia: Piranha solution). Production lines heat it further: according to one stripping patent, batch immersion typically runs at 120–150 °C and single-wafer spray at 170–250 °C; but above 170 °C, silicon nitride and silicon dioxide films are noticeably etched (US 8,940,103).
The most common reactive gas for plasma ashing is oxygen; fluorine-containing gases or forming gas with about 2% hydrogen in nitrogen are also used. Small amounts of photoresist left in trenches after ashing are removed by a “descum” step (Wikipedia: Plasma ashing).
How do the three methods compare? One table
| SPM (sulfuric acid + hydrogen peroxide) | Plasma ashing | Ozone water / ozone microbubbles | |
|---|---|---|---|
| Dry / wet | Wet | Dry (vacuum) | Wet |
| How it removes resist | Hot, strong oxidation breaks down and dissolves photoresist | Reactive oxygen atoms turn photoresist into gas that is pumped away | Ozone and OH radicals oxidize and decompose photoresist |
| Strengths | Fast, thorough, most production experience | No strong acid; wafers go in and come out dry | Little sulfuric acid; reverts to water and oxygen after reaction, low residue |
| Watch for | Large volumes of strong acid and high heat; excess heat etches silicon nitride and oxide; heavy waste treatment burden | May leave residue; crusted resist can burst if heated too fast; often needs a follow-up wet clean | Ozone is toxic and requires a sealed chamber, exhaust, destruction units and detectors; crusted resist is hard to remove with ordinary ozone water |
| Typical use | Primary wet strip, post-implant strip | First-pass removal of most photoresist | A direction for reducing strong acid use; ozone microbubbles are still in evaluation and adoption |
In practice, one method is rarely used alone: a common approach is ashing off most of the photoresist first, then cleaning the residue with a wet process (SPM or other chemistries). Ozone water and ozone microbubbles are seen as alternatives that cut sulfuric acid use and waste burden; for the principles, see OH radicals and microbubble cleaning.
Why is photoresist after ion implantation so hard to remove?
According to one ashing patent, this carbonized crust is about 200–2,000 Å (20–200 nm) thick, depending on the implanted species, voltage, dose and current; it is very difficult to dissolve in ordinary wet strippers (US 8,273,259).
Temperature rises too fast
The wafer heats up during ashing, and solvent in the underlying photoresist starts to vaporize.
Gas is trapped under the crust
The crust is impermeable, so vapor builds up beneath it and pressure keeps rising.
“Popping”
The pressure bursts through the crust, scattering fragments everywhere and leaving residue and defects that are hard to clean.
So it is processed in stages
First remove the crust slowly at a lower temperature (e.g., 120–160 °C), then raise the temperature to ash the underlying photoresist quickly.
Wet processes have countermeasures too: a patent notes that raising SPM temperature markedly improves removal of high-dose (e.g., above 1×10¹⁵ atoms/cm²) implanted photoresist, but then runs into film loss (US 8,940,103). Another direction is ozone microbubbles: Masayoshi Takahashi and colleagues at Japan's AIST found that adding microbubbles to ozone water removed high-dose implanted photoresist that ordinary ozone water and chemicals struggle to remove (Takahashi et al., 2015), and he regards microbubbles as a candidate technology for removing crusted photoresist in single-wafer cleaning without substrate loss (Takahashi, 2018).
How to choose? Ask these 4 questions first
Has the photoresist been through high-dose implantation?
Crusted photoresist is the hardest case; choose ashing that can run in stages, or combine with hot SPM, ozone microbubbles or similar methods, and watch closely for popping and residue.
What material is underneath?
Silicon nitride, silicon oxide, metals and low-k materials each have weaknesses: hot SPM etches films, and oxygen plasma can affect some low-k materials. Confirm the underlying layer before deciding on the method and temperature.
How clean does it need to be?
Advanced nodes have strict requirements for residue, particles and metal contamination; ashing is usually followed by a wet clean, so the whole sequence should be evaluated together.
What are your site's rules on strong acids and ozone?
SPM involves using, reclaiming and treating large volumes of sulfuric acid; ozone requires containment, exhaust, destruction and detection. Many fabs strictly limit ozone, so check before adopting it.
Further reading: for ozone water safety regulations, see What is ozone water?; for choosing ozone microbubble equipment, see how to choose a micro-nano bubble generator.
FAQ
What is photoresist stripping?
Photoresist stripping is the step that removes spent photoresist after lithography, etching or ion implantation. Photoresist is only a temporary template in the process and must be fully removed after each layer; chips have dozens of layers, so this step repeats dozens of times.
What is SPM, and why does it strip photoresist?
SPM is a mixture of concentrated sulfuric acid and hydrogen peroxide (known as Piranha solution), commonly about 3:1. Mixing releases a lot of heat, and it is highly oxidizing and corrosive, breaking down organics such as photoresist. Production lines usually heat it, but excessive temperature attacks silicon nitride and silicon oxide films.
How does plasma ashing differ from wet stripping?
Plasma ashing is dry: oxygen plasma in a vacuum chamber turns photoresist into gas that is pumped away, with no strong acid. Wet stripping uses SPM or other chemistries to break down and dissolve photoresist. In practice, ashing is often followed by a wet clean to remove the residue it leaves.
Why is photoresist hard to remove after ion implantation?
High-dose ions turn the photoresist surface into a carbonized crust that resists ordinary strippers. If ashing heats it too fast, solvent in the underlying resist vaporizes, gets trapped under the crust and eventually bursts, creating residue. So the crust is usually removed at low temperature first, then the temperature is raised to process the resist underneath.
Can ozone water replace SPM for photoresist stripping?
Ozone water is one way to cut sulfuric acid use, and research has confirmed that adding microbubbles increases ozone water's stripping rate and removes crusted post-implant photoresist; in one major chipmaker's evaluation, it was about 50% faster at the same ozone concentration (see the case study). Whether it can replace SPM depends on the photoresist type, underlying materials and throughput needs, along with proper ozone safety and exhaust handling, and should be evaluated on your actual process.
Source
- Wikipedia, “Photoresist”, 2026-10-23. Link
- Wikipedia, “Plasma ashing”, 2026-10-23. Link
- Wikipedia, “Piranha solution”, 2026-10-23. Link
- Google Patents, “US 8,940,103 B2 – Sequential stage mixing for single substrate strip processing”, 2026-10-23. Link
- Google Patents, “US 8,273,259 B1 – Ashing method”, 2026-10-23. Link
- Journal of Photopolymer Science and Technology, 28(2), 293–298, "Effect of Microbubbles on Ozonized Water for Photoresist Removal (Takahashi, Horibe, Matsuura, Tatera)", 2015-05-11. Link
- 表面と真空 (Vacuum and Surface Science), 61(2), 64–69, "Fundamental Properties of Microbubble in Semiconductor Cleaning Technology (Takahashi)", 2018-02-10. Link